B2B platform for R&D and prototyping. Outsource tests. Hire interim experts. Buy, rent or lease assets.

The website of I.revitalise uses cookies to improve your user experience.

+
Pitting Corrosion Testing

Pitting Corrosion Testing

Operator: Always included

The ASTM G 48 A/C/E test method and the ASTM G 46 test method.

Description

ASTM G 48 - Standard Test Method for pitting and crevice corrosion resistance of stainless steels and related alloys by the use of ferric chloride solution.
Method A—Ferric chloride pitting test.
Method C—Critical pitting temperature test for nickel-base and chromium-bearing alloys.
Method E—Critical pitting temperature test for stainless steels.
ASTM G 46 - Standard Recommended Practice for examination and evaluation of pitting corrosion.
This Owner can carry out almost all standard corrosion tests. It is also possible to perform corrosion testing on non-standardised products and test setups.

Quality labels

  • ISO 9001
  • EN 1090
  • EN 15085
  • EN ISO 3834
  • EN 13445